Gravure printing ink in the use of water-based ink, blocking is the most likely problems, mainly because of gravure printing ink poor compatibility, so once the operation is not appropriate, it is very easy to produce blocking. Plate blocking will lead to a series of print quality problems, such as pinholes on the surface of the print, small text lack of pen breaks, uneven ink colour, leakage of the bottom and other phenomena. Plate blocking causes and solutions are as follows.
(1) intermittent stopping stopping the plate, ink due to thinner volatilisation and dry solid in the mesh cavity. At this time, it is necessary to use one-to-one tools and cleaning agents to clean the printing plate, the letter of the contract to remove the printing plate, the use of organic solvents (ethyl acetate) to clean. Therefore, in the intermittent downtime, it is recommended to use the downtime without stopping the plate, so as to avoid the ink dry solid in the mesh cavity.
(2) The ink dries too fast and instantly dries in the mesh cavities. In this regard, first of all, you can add a small amount of slow drying agent in the ink, slow drying agent can prevent and slow down the ink drying time, to prevent the ink surface crusting, the general dosage is controlled at 3% to 5%; secondly, consider whether the thinner ratio is appropriate, the contract needs to be adjusted to adjust the ratio of the thinner, usually tea packaging printing environmental protection ink thinner alcohol and water ratios in the range of 1:1 to 4:1, but in the case of increasing the proportion of water Need to consider the amount of water, if the amount of water added too much, on the one hand, it will produce too many bubbles, on the other hand, it will lead to impermeable ink drying, so that the prints produce sticky dirty or ink anti-pull phenomenon.
(3) Ink viscosity is too high. At this time, the ink viscosity should be appropriately reduced, but need to take into account the printing speed and levelling. Because the ink viscosity is too low, it will produce too many bubbles, resulting in white spots on the surface of the print, print graphics too light in colour or fine lines and small text coarsening and other issues.
(4) The printing plate mesh is too shallow. At this time, should be appropriate to deepen the scale of the printing plate mesh, but need to consider the printing plate mesh is too deep when the quality of the problems that will occur, such as coarsening of the handwriting, fine text fuzzy, unclear patterns and other phenomena.