Common faults of laminating film and their solutions


Release time:2024-04-30

Laminating film is a common packaging material, widely used in food, medicine, electronic products and other fields. In the process of use, the composite film may appear some common failures, the following will introduce these failures and their solutions.

I. Common Failures

1. Bubble problem: Bubbles may appear in the laminated film, which is manifested as raised surface of the film or internal air bubbles.
2. wrinkle phenomenon: wrinkles appear on the surface of the composite film, affecting the appearance and performance.
3. Insufficient peeling strength: the adhesion between the layers of composite film is insufficient, and it is easy to delamination.
4. Shrinkage problem: Shrinkage phenomenon occurs during the processing or use of composite film, resulting in unstable product size.
5. Poor transparency: the transparency of the composite film is insufficient, affecting the display effect of the product.

Second, the solution

1. Bubble problem solution:


* Adjust the temperature, pressure and speed in the production process to ensure that the parameters match.
* Use high-quality raw materials to ensure that the surface of raw materials is free of defects.
* Optimise the lamination process, such as adjusting the amount and uniformity of glue application.
2. wrinkle phenomenon solution:


* Adjust the tension in the production process to ensure that the film is uniformly stressed in the lamination process.
* Optimise the film pre-treatment process, such as corona treatment or flame treatment.
* Use additives or auxiliaries with good anti-wrinkle performance.
3. Insufficient peel strength solution:


* Select suitable adhesive and laminating process to ensure the adhesion between layers.
* Surface treatment of raw materials to improve their adhesion ability.
* Adjust the temperature and pressure when laminating to ensure that the adhesive is fully cured.
4. Shrinkage problem solution:


* Select suitable material and thickness to improve the dimensional stability of the product.
* Adjust the temperature and speed during production to avoid excessive stretching and shrinkage.
* Use shrinkage inhibitors or stabilisers to reduce shrinkage.
5. Poor transparency solutions:


* Select raw materials and additives with high transparency.
* Optimise the laminating process to avoid turbidity or haze in the laminating process.
* Adjust the temperature and time during the production process to ensure that the materials are fully fused and crystallised.

In short, for the common failures of laminating film, it is necessary to comprehensively analyse and solve the problem from the aspects of raw materials, process and equipment. By optimising the production process and selecting suitable additives, the performance and quality of the composite film can be effectively improved.

 

Hubei Jinde Packaging Co., Ltd.

| “Preferred Supplier Of Color Printing Packaging Solutions”

Contact Us

Contact: Ms Zhang

Cell: +86 15807178126

E-mail: scarlette@jindepack.com

Add: Changxing Road No.2, Xiaonan Economic Development Zone, Xiaogan City,Hubei, China

%{tishi_zhanwei}%

Welcome to leave an online message, we will contact you promptly

%{tishi_zhanwei}%